WG glass wool (glass curtain wall) (Grade A)

Glass wool is made of natural minerals such as quartz sand, dolomite, borax and other inorganic materials, which are mixed according to specific process formula ratio requirements, hot-melted at 1360℃, and made into a series of products such as glass wool felt and glass wool board using advanced centrifugal fiber-forming technology.

32-64kg/m³

Operating temperature

≤0.039 at 70℃

density

Thermal conductivity

-18℃-232℃

Product Introduction

Mainly used as thermal insulation, fireproofing and heat insulation interior insulation material.

Application

Glass wool is made of natural minerals such as quartz sand, dolomite, borax and other inorganic materials, which are mixed according to specific process formula ratio requirements, hot-melted at 1360℃, and made into a series of products such as glass wool felt and glass wool board using advanced centrifugal fiber-forming technology.

Product Performance

Thermal insulation performance

Sound absorption performance

Environmental performance

Fire performance

The use of fine fibers increases the number of fibers, improves the insulation effect, and compared to 80K rock wool, 16~24KAclear can achieve equal or better insulation performance. It can reduce the weight of insulation materials by 70~80%, achieving significant lightweighting.

The fiber refinement technology improves the sound absorption performance and can improve the sound insulation performance.

No formaldehyde. No materials containing formaldehyde are used in the production process, achieving a comfortable indoor air environment. No odor. Due to the change of adhesive, the peculiar odor of glass wool and rock wool is also eliminated.

It uses basalt, dolomite and other main raw materials, and has extremely strong fireproof and heat-insulating properties.

Technical Parameters

Performance Project
Technical Parameters
Implementation Standards

Operating temperature range

-18°C to +232°C

GB/T 13350

Corrosion resistance

No chemical reaction

GB/T 13350

Average fiber diameter μm

5-8

GB/T 5480

Moisture content%

≤1.0

GB/T 16400

Moisture absorption rate%

≤5.0

GB/T 5480
Water repellency %
≥98
GB/T 10299

Bulk density (kg/m³)

32 40 48 56 64
GB/T 13350
Thermal load shrinkage temperature ℃

≥300 ≥350 ≥350 ≥350 ≥400

GB/T 13350

Combustion performance

Non-combustible materials
GB/T 13350

Thermal conductivity W/(m·k) Average temperature 70°C

≤0.042 ≤0.040 ≤0.040 ≤0.039 ≤0.039

GB/T 13350
Combustion performance grade

A-level

GB 8624

Slag ball content (particle size > 0.25mm)%

≤0.3

GB/T 5480